It would the vertical weld thickness,or the depth of the groove being welded.
In this case, 40mm.
These days, all codes have electronic versions, type in your query keywords in the search box, you'll end up with tons of answers & related explanations.
Thanks.
P.Goswami, P.Eng, IWE.