Tuesday, February 15, 2022

Re: [MW:32870] P91 - Repair Welding and PWHT

What is total holding time including repairs PWHT  and initial PWHT Holding time.

What was holding temperature?

Vishwas 

On Tue, 15 Feb 2022, 08:42 Sathish V P, <sathishvp86@gmail.com> wrote:
Dear All,

We have a scenario where the SA335P91 - Weld joint had 3 repairs and PWHT Cycles.

Is there any code reference to limit the number of repairs / PWHT in the P91 weld joints or what permissible times PWHT could be done on the same joint.

In this case - Pipe MOC - SA335 P91 - NPS 4 and 13.89mm thick.

Thanks,
Sathish

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACOF__aYi2PepJFn6Or2ubuCp0wj5R4TE_vAbYTrQ64Y8dZo0g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3PmMFxO17V_Fdjz5mr%3D-HTX2LC1pPzd-jUjQ03i_NBLdw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...