You described about circumferential weld not long seam
K.S.Unnikrishnan
Thanks and Regards,
Kollara
On 18-Feb-2022, at 7:24 AM, udaya bhaskar <dusroni@gmail.com> wrote:
Mr.Hany,Check do you've any client specification, if not follow the API1104 and the distance between the weld seams depends on application & technical data(i.e.,Dia of pipe,thk,Mat.grade,pressure ..........)On Tue, Feb 15, 2022 at 6:13 AM Hany Nabil <eng.hanynabil20@gmail.com> wrote:--Dear ExportsI have piping to fitting welding but always we have to keeping distance between two seam weldsSomebody said shall be 90 degree to be distance between two seam weld but I;m not sureSo, I would like to ask what is the distance between seam welds for the piping and mention the reference please ?Best Regards,Eng. Hany NabilSenior QA / QC Welding EngineerEmail: eng.hanynabil20@gmail.comEgypt Mobile: 002-01225622022This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmTgBzKWscEPP_mbPVb2WiiyYGLwD1OOZDjzwBLn4_OFAw%40mail.gmail.com.
----With RegardsUdaya bahaskar.D+919676270121
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RNjG_BNt5m92rjw1Sx7-Xco_vO-iXTXroXhHcOoZdmFsA%40mail.gmail.com.
Comments