Re: [MW:32942] CS to Inconel 625 Material _ Suitable Welding Consumable

NiCrFe2 for high temp & Creep service.  For ur combination ,it is better to use NiCrMo3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 23, 2022 at 9:29 AM Manikandan J <mechmani22@gmail.com> wrote:
Dear All,

What is the Suitable Consumable for CS to Inconel 625 Material for GTAW & SMAW Material.

Process : GTAW & SMAW

Regards,
Manikandan



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmNk3ySUGffFw_3pVtosNQj_4AS3S-w9HKS4Bud54qEbDQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMPcukaucDFmRft5O0dGmEhkorByVAx5qpT4KTjQGyd-A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...