Thursday, April 22, 2021

Re: [MW:32326] PMI for ASTM A105 Flanges

PMI will not work in this case...
You have to take samples for mechanical testing...
Tensile and Impact tests are essential for A105...

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Thu, Apr 22, 2021 at 8:12 AM Babur Khan <mbabur.bwp@gmail.com> wrote:
Dear Experts,
One of our contractor purposed PMI for ASTM A105 Flanges due to lake of inspection documents.
As my understanding PMI is suitable for HSLAS,
SS and DSS. For carbon Steel we can check if there is something happened im change of welding consumables for welding.
Please share your experience.

Babur Khan Lashari

Sent from my iPhone

Muhammad Babur Khan
Sent from my iPhone

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F2094BAB-A558-456E-9910-FD7962768B98%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUhP_3Qz88uikxfoPa3F418HU_jAAdQJa9%2BnthXaT27wcw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...