[MW:32278] Back Weld at Pressure vessel - U stamp

Dear Gentlemen,

   Good Evening, In our project Vessel joint thickness 10mm ,Process(GTAW+SAW),Single V joint 
They completed Welding ,Few days later during Inspection we observed , They have done Internal Welding of the shell, As per WPS its not shown 

Guys let me Know  its can Accepted or Rejected 

If Rejected , Please send Reference code standards

As per QW 402.5 Joints (Backing its non Essential ),Its mention Backing strip or also back welding 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/674e4919-ecd5-46bf-84ec-3fd22eed8280n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS