Re: [MW:32264] Tube welding design

GTAW
Single V..

Regards

Prem Nautiyal 


On Thu, 15 Apr 2021, 19:27 EmaD FaRaHanI, <emad.farahani@gmail.com> wrote:
Dear all,
Tube A210 welding with GTAW or SMAW with thickness 5.5mm, obviously no access to the inside of the pipe. 
What is your suggestion? square butt or single v?

Thanks,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJFa2e_1dMQ3hiriryK7YYe5iuZQgP3S6UxVhugKEfL16w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEP2HKBjA8OBd887zBH_OJKYW7CoD3VJjA9QrXv5LgNzVPA_Qg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...