Dear we have in our previous projectClad material in AlHosan gas Abudhabi and we found there is no issue in that material go a headRegardsPravean--On Wed, 14 Apr, 2021, 11:42 am PK M, <pkmqaqc@gmail.com> wrote:--Hi experts,
CLAD MATERIALS -WELDING
We have the following Clad Pipe and we are preparing WPS /PQR to weld this SPOOL.
As I know we need to use ERNiCrMo3 / 7018-1 Combination (if GTAW+SMAW) to Complete weld.
But if anyone is having experience with this, please advise whether we will go with
GTAW - ER NiCrMo3 ( Root & Hot )
SMAW – E7018-1 (Balance Filling /Capping).
Please Explain any troubles may have happened regarding dilution or not.
Need Aramco and International code reference? If any one has a sample WPS/PQR Please share with us.
Any corrosion test or NDT
Waiting for your scientific and specific reply.
Thanks in Advance.
Pkm
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_neYBsYs0Ly8VaMw5SMMw_ueaaAZM4QQs7B_KryHZkjhRQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANO0gODQN_xqMn6tj-oMEv8zh98k9%3DmtUZa-yMDUuFrSxqEncg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nfSkjeBzTeV9DijMOK6G-PttF0uA6b%2B-s8kji%3Dg1%2BmWfw%40mail.gmail.com.
Comments