Dear Jacob,
Please refer ASME section IX article 1 to 4Article 2 related to PQR & WPS
Please understand the essential/non essential variables as well as supplementary variables. Inaddtion to that you can WPS formats in article 2
Please go through from QW 402 onwards
Best Regards 
Sayeed




Sent from my iPhone

On Apr 16, 2021, at 7:16 PM, Jacob Basili <yousabcreator@gmail.com> wrote:

I am just a fresh graduated person and I took courses for PT, VT, MT and RT and I wanna learn now how to make WPS in a shortest time. Any one have a way, please !! 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7d1ec32e-8697-4171-a4a2-e76f8e3b28c6n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...