Thursday, April 15, 2021

[MW:32247] Required sample copy of welding procedure Specification for Galvanized pipe welding..

Respected experts,

If any have sample copy of approved welding procedure with PQR for Galvanized pipe welding.please share me for reference..

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKKH_q2-DUfdTQ9T6T%2BOXSjAveADRzdhM8ci4MSugA%2B6xw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...