Re: [MW:32250] PWHT REQUIERMENT FOR PIPING AND PIPELINE

As we know, After ASME B31.3 2012 editions, the PWHT requirements for greater than 20mm thick has been changed to 95 Deg Preheat for all thickness P.No1 material.

 

Though its excepted from latest editions, pl check the following for PWHT requirements

 

1.    Pl check the Applicable ASME edition as per your contract

2.    Pl check do u have qualified WPS/PQR without PWHT for higher thickness

 

Many clients specify in contract to follow 2012 edition, to perform PWHT for greater than 20mm thick. This is to avoid  the potential risk involved when higher thickness pipe welding at a later stage. 


Thanks and Regards

Rameshkannan D

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"


On Wed, Apr 14, 2021 at 8:08 PM pravean ashok <gujulapravean@gmail.com> wrote:
Yes brother compulsory you have to do preheating but you need to maintain the temperature so my recommendation is better for coil induction coil heating is good to maintain the temperature 

On Wed, 14 Apr, 2021, 7:55 am QA/QC, <adnanziad49@gmail.com> wrote:
Dear masters 

we want to weld a pipeline api 5l x70 thhikness 28 mm so we want to know the requierement of PWHT CODE API 1104 

AND ALSO FOR A333 GR 6 THICKNESS 45 MM CODE B31.3  . PWHT REQUIERMENT 

CAN ANYONE CLARIFY IT FOR ME 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1123834c-5b79-4fd8-8864-0deaf7c0e3fcn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANO0gOA-fhviVkNiDBO%2BJbYZL6VFePdDzS_N-fAiRfhovazyzA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcHyCKWLO8j%3DfmqZzXXmkDfG8LEQ5VR3XM3taOos9miCBA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...