Re: [MW:32297] Re: Back Weld at Pressure vessel - U stamp

Dear 

 As per ASMe sec IX QW 402  - Joint design - GTAW - Backing - With/Without 

GTAW - QW 402.5- Addition of  backing is Non essential variable.)

if Both (Backing - With/Without  )  must be addressed in your WPS then there is no issue to weld 

Regards
Pravean

On Mon, 19 Apr, 2021, 6:05 pm Ramesh, <rameshkannandevaraj@gmail.com> wrote:

Don't not confuse with production weld and repair welds

 

Though its single sided weld as per WPS for your production ,  when repair comes at root what you do ? ( presuming accessible at root side )

 

For repair, your weld metal is backing material, so any welder qualified with backing or without backing can repair in your case. 


Thanks and Regards

Rameshkannan D

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"




On Mon, Apr 19, 2021 at 5:31 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Dear Samkar

May I know what is your concern now ?

On Mon, Apr 19, 2021 at 3:51 PM sankar bombay <sankar.bombay@gmail.com> wrote:
For GTAW Welder QW-402.4 Deleting of backing is essential Variable 
Addition of backing they have not mention 

On Mon, Apr 19, 2021 at 2:19 PM Ramesh <rameshkannandevaraj@gmail.com> wrote:

Seems weld repair carried out at the root side. Whether your repair carried out as per approved repair procedure ? 

 

With Backing or without backing is essential for welders, not for procedures !

unless there are any specific requirements from the client / inaccessible area for root welding.


Thanks and Regards

Rameshkannan D

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"




On Mon, Apr 19, 2021 at 1:09 PM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
Is  that WPS  addressing - 
 QW 402  - Joint design - GTAW - Backing - With/Without 
(Ref - QW256- GTAW - QW 402.5- Addition of  backing is Non essential variable.)

if Both (Backing - With/Without  )  is addressed( which  like  normally is  addressed), then there is no issue at  all .

Eg-

QW 402-

Backing: With/Without                                                                         

Root spacing: As per piping fabrication drawing                                                                                                          

Backing Material (Type): Yes (Metal)

1. Metal -        2. Non-fusing Metal      

3.   Nonmetallic NA   4. Others 

The matter is to  be resolved  amicably . Meet QAC  In charge along with Welding Engineer, Manufacturing Responsible. Explain him the details . 
It shall be acceptable.


Regards

On Monday, April 19, 2021 at 7:20:46 AM UTC+4 sankar krishnan wrote:
Dear Gentlemen,

   Good Evening, In our project Vessel joint thickness 10mm ,Process(GTAW+SAW),Single V joint 
They completed Welding ,Few days later during Inspection we observed , They have done Internal Welding of the shell, As per WPS its not shown 

Guys let me Know  its can Accepted or Rejected 

If Rejected , Please send Reference code standards

As per QW 402.5 Joints (Backing its non Essential ),Its mention Backing strip or also back welding 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/960d2caa-6684-4216-b79d-6eb48095898cn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcGxuHhMRmyXeJobuwT02Mx8KudViGRskgQuiJNRr6ED%3Dw%40mail.gmail.com.


--
shankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyDEeYx%2Bjddw7_cQ_J1A7u3Op1N-pk9t%2BcAh7LDxXym8AAA0g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3McUQS%2B%3DqRQppxd1B0SUSi9_P3ycAaUPyMU%2B8E93FpRAA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcH%3DqrTAWpycfZ7nUjMYNX7%2B0MwFcBzzNNUXUXVx4KEkvQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANO0gODPHXtP0YfHo0nEqarjR36OEq5aVFeU_70Wp4RxABoXng%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...