Re: [MW:32235] Weld Quality Inspection

For a Fillet weld, it is based on the Throat size and Leg size and the required profile as convex or concave as Applicable

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 14 April, 2021, 07:58:49 am IST, Harish Kannepalli <harishkannepalli@gmail.com> wrote:


Hi,
    Please follow ISO 5817 for weld quality levels. However this has to be documented in your or end user SOP.

Regards,
Harish Kumar

On Wed, 14 Apr 2021, 07:55 Amit Singh, <amit086@gmail.com> wrote:
Dear Experts,

What is the acceptable weld bead reinforcement and allowable penetration in the GMAW welding process? Any specific code for structural welding. Please suggest.

Joint design- Fillet Type
Plate thickness- 8mm to 32mm
Material Grade- IS2062 E350C

Thank you in advance.

Regards,

Amit Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKBY_CEcnyT2Z_2Cnu3yFT_LYBhJRwJ%3Dy1Dp2rzq9YLm4PUVow%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE4SttFQPkMa-a2SoyqS_sGG-BpBumZmVg8Dfx3kZUNYawfRcA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...