Re: [MW:32256] welding api 5l x52 with x60

API 1104 permits to weld the below but check your specifications as some specifications like shell DEP do not permit to weld high thickness above 25mm and pipe to fittings using Cellulosic electrode which commonly used for Pipeline welding.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 15 April, 2021, 01:08:03 pm IST, QA/QC <adnanziad49@gmail.com> wrote:


Dear master 
i have a approved wps for welding api 5l x52  pipeline and i want to weld a anchor flange x60 is the wps cover it or we should requlaify it again 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c82adcc6-aec4-4acc-9815-966de7fd1a23n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...