it is better to do it in black condition including base material to ensure no leakage.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Tue, Apr 20, 2021 at 8:32 AM Alcindo Jardim <alcindoj@gmail.com> wrote:
NoYou must take off the paint of the weld....--Em seg, 19 de abr de 2021 09:40, Manish Kumar <mkmkr431@gmail.com> escreveu:Dear Sir,--Please advise for pneumatic testing, if Welding joint is covered from painting.Can we witness for pneumatic testing of weld.Please advise in this issue.Regards
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k4AmGm8yvxiw2NNC0%2B%3DfRAQZGqq6wVCdBtSn5N4h3ugkQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANT8xKR_6rCiB97prrx654qdyHCoXt2Jqo-01cXQ1-%2Bo%3DHZprA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM8CVbD7eb%2BKEqK%2BA1rq7%2BFuyQNDHWC1fT6nKVZiVmM9A%40mail.gmail.com.
Comments