Thursday, January 30, 2020

Re: [MW:30438] PWHT ( extra requirement. (2 more cycles))

Please Sir,

Describe me how I can  mention in WPS.

On Thursday, January 30, 2020 at 10:28:02 AM UTC+5:30, kannayeram gnanapandithan wrote:
Ref 2018 edition, temperature range is changed. Your client is okay

On Wed, 29 Jan 2020 7:35 pm K K, <kara...@gmail.com> wrote:
Dear Experts,

I need your feed back urgently.

With reference to above subject PWHT requirements for  A 335 Gr P11 to A 335 P11.
As per ASME B31.3 and for CLG units.

1) First WPS Base metal thickens - 5.0 to 62.00mm

2) Second WPS Base metal thickens - 1.5mm to 12.00mm


As per B31.3 - PWHT require as per Table - 331.1.1 for P4.

And as per CLG - PWHT Require  - (704-760C), 1 hour per inch (25 mm) of thickness, 2 hours minimum.
My client give a comments as below.

1)  Extra cycles for repairs acc. to project spec.in PQR.
2) Soaking time must include possible repairs. In addition to the extra requirement. (2 more cycles).
3) Soaking time according to quoted specification (2h) and anticipating 2 repair cycle. So 6h. Coupons for minimum and maximum temperature (simulated test).

I couldn't understanding the above comments. 

Can you please explain me in detail for PWHT  requirements, Time calculation, how i can calculate Hour's. 
And how i can mentioned in both WPS.

Thanks in advance.

Thanks & Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/99b3941f-7e90-4187-8eab-2317440f5339%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aed1d872-e362-400f-bd69-6935ce872822%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...