I have been in several ASME audits for recertification (Joint Review), with Designers U, S and R of the National Board, with the Authorized Inspection Agencies: OneCis and HSB GS and certainly non-Dstructive Testing Procedures are presented in these audits, such as VT, PT and others, and in none of the cases did these procedures carry signatures of a Level III of ASNT.
He estado en varias auditorias ASME para recertificación (Joint Review), con Designadores U, S y R del National Board, con las Agencias de Inspección Autorizadas: OneCis y HSB GS y ciertamente se presentan Procedimientos de Pruebas No Dstructivas en estas auditorias, como son VT, PT y otros más, y en ninguno de los casos estos procedimientos llevaron firmas de un Nivel III de ASNT.

El jue., 9 ene. 2020 a las 5:13, Kannayeram Gnanapandithan (<kgpandithan@gmail.com>) escribió:
Mainly required for stamp holders whether it is coded or non coded. All NDT procedure and personal are to be certified/ approved by Level 3. 

On Thu, 9 Jan 2020 2:38 pm chiluka venkatramulu, <ramuluchiluka@gmail.com> wrote:
Dear All,
Pl clarify whether  it is required NDT Level-III approvals for all NDT procedures? or required only for coded vessels.
Pl specify the code requirement.

Thanks & Regards,
Venkatramulu CH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHdFX5ePVY4%2B5GB9pFh4ZGGoRu0ntafcZrkCw17XMdkrQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM4VRRfT57r-k4nyacd9PjZftwsP1V38bMVu%2B3swydHZg%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurK-ubnnur2t%2BsL1bKa%2BEWc_DNZ8%2B04RV4L3yV0CiLc-eQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...