Fw: [MW:30435] Re: Welding of S32750 super Duplex Steel

Resending ..
The recomended GTAW filler alloy is SFA 5.9 ER2594 & not ER2507 
Inconvenience is regretted. 
Thanks Amitabh

----- Forwarded Message -----
From: Amitabh Bhattacharya <amitabh_3@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, January 28, 2020, 09:36:56 AM EST
Subject: Re: [MW:30429] Re: Welding of S32750 super Duplex Steel

Hello
SA790 UNS S32750 is the specification for Super Duplex Pipes & Tubes . 

Therfore use of ER2507 filler alloy  will help in Ferrite-Austenite balance . 

Weld metal producing PREN> 40  is requirement for Corrosion properties for such joints.. 

I would use the attached brochure for further studies & weld alloy selection.
Hope this helps 
Amitabh 

On Tuesday, January 28, 2020, 03:29:19 AM EST, Bien_ND / weldinginspections.net <bck055@gmail.com> wrote:


I recommend to select AWS A 5.9 ER2209 or ER309LMo.
Refer to API RP 582 Table A.3.


On Saturday, January 25, 2020 at 4:51:48 PM UTC+7, VIshaL wrote:
Dear Experts,

One of our project we have to weld material with GTAW process as per following.

1. SA 790 UNS S32750 to SA 780 UNS S32750

2. SA 790 UNS S32750 to SA 240 Gr. 316L

Request you to please confirm suitable filler wire Grade as well as any special care require during welding.

Thanks in advance.

VIshaL SUTHAR


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/11253781-f179-4a53-acbd-27309ea7a4d2%40googlegroups.com
.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...