Please Sir,

Describe me how I can  mention in WPS.

On Thursday, January 30, 2020 at 10:28:02 AM UTC+5:30, kannayeram gnanapandithan wrote:
Ref 2018 edition, temperature range is changed. Your client is okay

On Wed, 29 Jan 2020 7:35 pm K K, <kara...@gmail.com> wrote:
Dear Experts,

I need your feed back urgently.

With reference to above subject PWHT requirements for  A 335 Gr P11 to A 335 P11.
As per ASME B31.3 and for CLG units.

1) First WPS Base metal thickens - 5.0 to 62.00mm

2) Second WPS Base metal thickens - 1.5mm to 12.00mm


As per B31.3 - PWHT require as per Table - 331.1.1 for P4.

And as per CLG - PWHT Require  - (704-760C), 1 hour per inch (25 mm) of thickness, 2 hours minimum.
My client give a comments as below.

1)  Extra cycles for repairs acc. to project spec.in PQR.
2) Soaking time must include possible repairs. In addition to the extra requirement. (2 more cycles).
3) Soaking time according to quoted specification (2h) and anticipating 2 repair cycle. So 6h. Coupons for minimum and maximum temperature (simulated test).

I couldn't understanding the above comments. 

Can you please explain me in detail for PWHT  requirements, Time calculation, how i can calculate Hour's. 
And how i can mentioned in both WPS.

Thanks in advance.

Thanks & Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/99b3941f-7e90-4187-8eab-2317440f5339%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aed1d872-e362-400f-bd69-6935ce872822%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...