Hi,

Efficiency of SMAW process is ~ 60-65%
Hence multiply the E6013 quantities (Kg) procured/ consumed by 0.4, to arrive at apprx wastage qty.

Regards,
Kiran
+966 572 416 045

On Sat, 25 Jan 2020, 08:41 Dinesh Somwanshi, <som.din@gmail.com> wrote:
Dear, 


Calculate the weight of entire electrode.

calculate weight stubborn electrode .

Deduction of both multiplied number of electrodes will give correct answer.

Regards

Dinesh

On Sat, Jan 25, 2020, 09:27 Sfmech <sharjeelfaiz@gmail.com> wrote:
Hello, is there any method to find weight of scrap electrodes, approximately. The electrodes are 6013 and are placed in a heap.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d1bca86c-aef6-4e98-aa3a-822914ac1829%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrVU2g7y7doi0s8Y%2BNuQQZRaZp%2BqG6ZArO1vAHs9bAobjQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD6_R_7M6wSAHqA%2Bt%3DL_QNibTQYVamio3zW5Ctjr6mDJSRU5Pw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...