Pls. find attached file.

Vào Th 5, 16 thg 1, 2020 vào lúc 10:33 Rishikesh Kumar
<rishikr06@gmail.com> đã viết:
>
> it is recommended to use the long seam weld shall be 90 to 180 degree orientation between two pipes. it helps to restrict crack propagation during failure.
>
> On Wed, Jan 15, 2020 at 4:50 PM Durgesh <durgesh.gaonkar@galiakotwala.in> wrote:
>>
>> please refer attached sketch for better understanding.,
>>
>> Pleas suggest permissible welding procedure with reference ASME standard.
>>
>> --
>> https://materials-welding.blogspot.com/
>> https://www.linkedin.com/groups/122787
>> ---
>> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e8c953fc-6602-4c81-9ccc-329d270235a7%40googlegroups.com.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEXs1KqXmuT6u6a7SJ_dES2LPX9j7i9mxpN%3DBy%3Db7n9bu1j39w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFrs4mW951CjMWvVVTjfAtWUW8D6xteQgq0wSButicsSDo%3DXOA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...