Dear sir,

Incoloy 617,   Need to maintain underpass strictly to 125 degrees.

PWHT may need if your service temperature exceeds 550 deg centigrade.

regards

Dinesh


On Tue, Jan 14, 2020, 14:39 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,
Go with ENiCrFe-2 (Incoweld A) or ENiCrCoMo3 (Inconel 617). No PWHT needed. You may preheat up to maximum of 75 degree Celsius.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282

E-mail : karthik6684@yahoo.com



On Tuesday, January 14, 2020, 03:51:56 PM GMT+7, <tuanpvecc@gmail.com> wrote:


Dear Experts 
Please suggest a good welding parameter for HP modification (25Cr-35Ni-0.1C+Nb) Material 
Welding consumable, PWHT if need.

Thank you 

N.A. Tuan


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/525e8e0a-6c8b-4f00-bc35-f83b20bbb085%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/105142528.7421479.1578992924882%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrXOu8ua%3D2iLgsRkE1pfvZQv8eYytFMzWGPYY5zEeSuj7g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...