Hi,
Go with ENiCrFe-2 (Incoweld A) or ENiCrCoMo3 (Inconel 617). No PWHT needed. You may preheat up to maximum of 75 degree Celsius.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282

E-mail : karthik6684@yahoo.com



On Tuesday, January 14, 2020, 03:51:56 PM GMT+7, <tuanpvecc@gmail.com> wrote:


Dear Experts 
Please suggest a good welding parameter for HP modification (25Cr-35Ni-0.1C+Nb) Material 
Welding consumable, PWHT if need.

Thank you 

N.A. Tuan


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/525e8e0a-6c8b-4f00-bc35-f83b20bbb085%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...