Wednesday, January 1, 2020

Re: [MW:30339] Re: P8 material limit of as per QW-403.6

As per QW-403.6, minimum base metal thickness qualified is T/2 i.e. 3mm & max. thk qualified is 2T i.e. 12 mm

On Mon, Dec 30, 2019 at 11:05 AM JAYAPAL DHAKSHNAMOORTHY <jmoorthy191@gmail.com> wrote:
  Dear experts,

I have qualified PQR of Thickness-6mm (P8G1) Austenitic stainless steel, & What is the minimum and max.thickness qualified  as Per QW-403.6.in WPS (for Impact).

Regards,
DHAKSHNAMOORTHY.J

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHHcqJdo7f3JVp4vAkH-77ucP9Gt4Z4uSVNmsM0o%3DfTr72cuXQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_ePWuxnZMQRx4b7tJn7fpVMAh4xyvxGxGpniE7Kv6rRC9A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...