Friday, January 31, 2020

Re: Fw: [MW:30441] Re: Welding of S32750 super Duplex Steel

Dear Sir,

Thank you very much for your valued reply.

Same is applicable for  SA 790 UNS S32750 to SA 240 Gr. 316L welding?

Please confirm.

On Thu, Jan 30, 2020 at 10:27 AM 'Amitabh Bhattacharya' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Resending ..
The recomended GTAW filler alloy is SFA 5.9 ER2594 & not ER2507 
Inconvenience is regretted. 
Thanks Amitabh

----- Forwarded Message -----
From: Amitabh Bhattacharya <amitabh_3@yahoo.com>
Sent: Tuesday, January 28, 2020, 09:36:56 AM EST
Subject: Re: [MW:30429] Re: Welding of S32750 super Duplex Steel

Hello
SA790 UNS S32750 is the specification for Super Duplex Pipes & Tubes . 

Therfore use of ER2507 filler alloy  will help in Ferrite-Austenite balance . 

Weld metal producing PREN> 40  is requirement for Corrosion properties for such joints.. 

I would use the attached brochure for further studies & weld alloy selection.
Hope this helps 
Amitabh 

On Tuesday, January 28, 2020, 03:29:19 AM EST, Bien_ND / weldinginspections.net <bck055@gmail.com> wrote:


I recommend to select AWS A 5.9 ER2209 or ER309LMo.
Refer to API RP 582 Table A.3.


On Saturday, January 25, 2020 at 4:51:48 PM UTC+7, VIshaL wrote:
Dear Experts,

One of our project we have to weld material with GTAW process as per following.

1. SA 790 UNS S32750 to SA 780 UNS S32750

2. SA 790 UNS S32750 to SA 240 Gr. 316L

Request you to please confirm suitable filler wire Grade as well as any special care require during welding.

Thanks in advance.

VIshaL SUTHAR


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/11253781-f179-4a53-acbd-27309ea7a4d2%40googlegroups.com
.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/362492790.1048873.1580318276764%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOZ%2B%2BqB7_7cUz7K2fmTGzbNhXYyEnzLtUs_Nqo2cA9Vy02jmqQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...