Monday, August 12, 2019

Re: Re: [MW:29948] Electrode expiry

Hi,

Electrode expiry, which is shelf life comes with manufacturing recommendations, but still some debate asking that ''whether its a food item to have expiry'' its not but it has shelf life which may differ 3 or 4 years as per manufacturer recommendations, and can be continued if stored in proper condition if your manufacturer accepts.

So at any case check the manufacturer recommendation and if exceed take a concurrnece from manufacturer and satisfy your client with continous proper storage records, because in any case of serious or pattern defects, before the question arises, have a proof, this shall be ongoing observation as a part of quality focus assesments.

Below is one of the australian manufacturer for electrodes, where i had to concur as proactive.


Regards,

Muneeb.

Date: 2019-08-12 15:20
Subject: Re: [MW:29943] Electrode expiry


Supplier recommending for 6 years.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*



On Mon, Aug 12, 2019 at 1:11 PM surya singh <surya8031@gmail.com> wrote:
Dear Experts, 

As per standards how many year after vacuum pack electrode expiry  

Regards

VINOD.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BfkJkskQLEUi6J_GZLbhXH3TfukHkkPzTn1dFfVYDyE5sc4gg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrXJ%2BCKBt6q-cAQWhWDgPw8Yi3PmUvEZvpS_wDpCbgApeA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...