Re: [MW:30008] Requirement of double Normalizing of SA-516 Gr.70

Why intermediate Normalizing required???. 

On Fri, 30 Aug 2019 12:29 pm 'Prakash Hegde' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi!
With multiple normalising.UTS gets deteoriates
Accordingly  ddelivery condition.of.plate.you req UTS on higher side than min requirement
Ii) Generaly for highet.thick weld.seam multiple Normalising.ll.reduce UTS as such Normalising criteria.is not.addressed in.Sec IX.or.Div 1 of ASME
THATS why most of the designer recomend Crown.n Petal.for higher thk.Dends
Regards
Hegde


On Fri, 30 Aug 2019 at 11:51, Jayesh Parekh
In our recent project i encounter one problem.

Material Grade : SA-516 Gr.70 Supply condition : Normalized
Dished end : Ellipsodial
Thickness : 45 mm
Forming process : Cold forming
Dished end have one cordal seam
Impact required at : -46 deg. C
so during cold forming vendor need one intermediate normalizing. and as per client requirement one more normalizing performed after complete dished end forming. So, total 2 time normalizing have to perform.

So, my question is ; 
(1) During plate order i have to take 2 normalizing cycle simulation ? Yes Or No? With Reason
(2) May I take benefit of Clause UCS-85 (i) of ASME sec-8 Div.1?
(3) Is same clause applicable for welding?
(4) And If i will perform double normalizing then I have to simply double the normalizing time or 2 separate normalizing i have to perform?
(5) What will be effect on weld and base material after 2 time Normalizing?
(6) if any one encountered such issues . please help to solve 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f9744a58-4c34-4c96-93f8-ff304e519db5%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/177254843.162832.1567147604899%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOV2bSEXEW-LEx%3DwQES%2BaqPVkoraRr%3DUY4vrTP9Ht256g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...