Wednesday, August 28, 2019

Re: [MW:30004] About humidity.

Dear All,

Pl note that, "SAND" is now prohibited in almost all around the world for blasting. 

We shall not used this term. 

"Blasting" is enough to understand and communicate. 

Some answers I saw given " it depends on Painting scheme" but the question was regarding Blasting not painting. 

For blasting RH shall be 60 or below. 

Regards.

On Thu, 22 Aug 2019, 09:24 Minhas Arshad, <minhasarshadm08@gmail.com> wrote:
Dear Experts,

I would like to ask from experts, how much himidity and dew point is allow for sand blasting Sa 2.5 in cloudy condition? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOHF6tt0SeQON2Jgm9sm0UC0NbkLmOwrhEfbTjq5-yT9q_CNA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEzKD3K6POSSXMN93tgifzbEMECbFYEtb4mJFk5CJ6041WKRwA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...