Sunday, August 25, 2019

Re: [MW:29989] WPS


As per your WPS,  Base material is API 5L X52  (  P No. - 01 Gr No. -01)
you need to weld for A106 ( P No.-01, Gr No -01) to A105 ( P No.-01, Gr. No.-02).

P No  is same  But Gr No is different... you cant use this WPS for proposed material.


Thanks & Regards,

Mani
QA/QC - Welding & Painting  



On Fri, Aug 23, 2019 at 7:18 AM tuscano09@gmail.com <tuscano09@gmail.com> wrote:
dear all,

can I use the attached WPS for A106 pipe and A105 pipe fittings?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08f4d0ee-d589-40b1-af5f-6889f66ce8a3%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOZuskowfPUbhpdKKv3BeS-00rK1eoH19Gks6m-J_v7XOa%2BM5Q%40mail.gmail.com.

No comments:

[MW:35692]