Yes!
WPS -------> P1 with P1
SA 106 Gr B is P1
SA 105 is P1
Regards!

El jue., 22 de agosto de 2019 11:18 p. m., tuscano09@gmail.com <tuscano09@gmail.com> escribió:
dear all,

can I use the attached WPS for A106 pipe and A105 pipe fittings?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08f4d0ee-d589-40b1-af5f-6889f66ce8a3%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJsteYNkT0mSZWhVF2tLKgEYnyReyPR7noMo66%3Dck7nRw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...