Not necessarily . Only pwht cycle. If dish is made of petal or any welding involved and same WPS , then u have to simulate all Heatreatment.
On Mon, 12 Aug 2019 3:44 pm chiluka venkatramulu, <ramuluchiluka@gmail.com> wrote:
Dear All,--Pl clarify the below.One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
- Dishends Normalising-2 cycle.
- PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?OROnly two normalising cycles are enough?Regards,Venkatramulu
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdGvDLB4C3Y24JY-HL4JW2%3DC%2BUuXnw8sFhsPDo6-i0sKSg%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePkc%3D%2B9SvYCosc%3D%3DKfkrmMNKLSbxq9fuxKxXpg6PkQ%3DYA%40mail.gmail.com.
Comments