WPS with PWHT is enough, since your dished end is in single piece (no welds).
you might include normalizing cycle only when any of the weld also under go normalizing (e..g dished end with weld)
On Mon, 12 Aug 2019 at 15:44, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,--Pl clarify the below.One of vessel under fabrication will under go the fallowing heat treatments. (Material-516 G 70, shell-63 mm, dish end -75mm, dish end in one piece only)
- Dishends Normalising-2 cycle.
- PWHT for whole vessel.
Now shall I need to do all three heat treatment cycles to qualify WPS?OROnly two normalising cycles are enough?Regards,Venkatramulu
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnzM_%2BuDh3cpNs944%3DYoyH%2BNP2ECHAcCTVyBqmxxR6ORg%40mail.gmail.com.
Comments