Tuesday, August 6, 2019

Re: [MW:29932] Welder qualification with process

Hi,

Please find below the extraction of diameter limits as per QW 452.3. If you qualified with the test coupon of OD 27/8"(73mm) then you can use them for both GTAW and SMAW. But if your test specimen is 6"OD for WQT of GTAW+SMAW (its qualified for minimum 27/8"(73mm and over) . If this case, you can not use SMAW for OD 2" of production welds.






Thanks& Regards,

 
(Karthik)


Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthik6684@yahoo.com







On Tuesday, August 6, 2019, 08:35:11 PM GMT+7, 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:





Dear Kartik sir,
Our client is opposing that; the welder is not qualified for SMAW in 2" NPS.

Regards 
Sangram 

Sent from my iPhone

On 06-Aug-2019, at 7:25 AM, 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:

> Hi,
> Yes. He can. 
> change in weld metal deposit more than he qualified only is an essential variable. Base metal thickness is not an essential variable for welder qualifications.
> (In your case for GTAW, maximum weld metal deposit thickness is restricted to the welder qualified for maximum thickness in 1" pipe)
>
> Thanks& Regards,
>
>  
> (Karthik)
>
>
> Karthikeyan.S
>
> QA/QC Manager
> Agon Pacific Co.,Ltd.
> M: +66-655-174-397, +66-892-512-282
>
> E-mail : karthik6684@yahoo.com
>
>
>
>
>
>  
>  
>  On Tuesday, August 6, 2019, 11:03:39 AM GMT+7, 'Sangram' via Materials & Welding <materials-welding@googlegroups.com> wrote:
>
>
>
>
>
> Dear experts
> Please give me your valuable feedback with code reference.
> A) One welder is qualified with dia 1" & above with GTAW(11mm)
> B) Same welder also qualified with 2 7/8 & above with GTAW + SMAW (7.5 mm Gtaw + max to be welded smaw )
> My question:
> Can this welder welded any 2" joint which thickness is more than 11mm by using GTAW+SMAW process ??
>
> Regards
> Sangram
>
> Sent from my iPhone
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/E4DEF482-CEE0-4A77-A796-AA166751B51E%40yahoo.com.
>
>
>
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1475311395.1335627.1565065529216%40mail.yahoo.com.
>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/47F0D7B2-05EC-4A3E-A95C-3B10FE9130FB%40yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1598714282.1456723.1565101434406%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...