Re: [MW:29918] Impact testing as per ASME B31.3

Check consumables are impact tested at room temperature. That's enough

On Fri, 2 Aug 2019 7:24 pm 'anand gupta' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
As per code for high temp impact test no need. 
Impact need for low temp only. 

Regards 
A p gupta 


On Fri, 2 Aug 2019 at 13:34, Khaled lamraoui
Dear experts.    I need your help please.  I have sa 335 p91 as base material used in power plant does this require impact test for preparation of pQR or not?        Ps: used for high temperature applications 600 degree. Can you please give a detailed explanation.              Khaled lamraoui.         


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/88a57bae-9e31-4ebc-8c66-1ec9124eb25f%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/194641271.359695.1564750983528%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOnnep8Rp7jX1Rthimkwmvsw1a1boH9T1v910TxLq7WfA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...