Sunday, August 25, 2019

[MW:29989] Boiler without S Stamp delivered to site

Dear experts 

 In our project we received Utility Boiler without S Stamp in Name Plate . Contractor response is hydro test will be done with AI involvement and final stamping will be done .
 
 But manufacturer supplied MDR documents signed by AI , certified with S stamp mentioning shop hydro test , thk , dimension details all.

 My query , if MDR is stating S stamp , why it was not stamped in Name plate at shop and delivered to site.
 
Thanks & Regards
Abraham 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOsuTKndp4%2BW0N%2BtsNJ2cOzdsGswgGJiHLd3wdX0GKWtmEQrZg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...