Απ: [MW:29987] WPS QUERY

If no impact test is required you can

Εστάλη από το Huawei κινητό μου


-------- Αρχικό μήνυμα --------
Θέμα: [MW:29976] WPS QUERY
Από: prabhu
Προς: Materials & Welding
Κοιν.:

Hi experst,

I have qualified WPS of P1 G2 (grade LCC) can I use this WPS to weld P1 G1 (grade LCB) material.

I yes with which clause and if not why not?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9209ad6e-56c5-407c-8f24-23d6568c4d53%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/-a8cgiw-rutiuh-nbx7ok-uus87o-p0bihb-imgqbp-m3ntp63y9w5i-x86296-u0pvqx8ooxsstolnlnvmnyrnhkx3s6yska2k-e3mhjir8m7pwcej3u0wxdnvh-gnhaoh-45z3ti-vqnp4y-svtorsrygym8.1566559172170%40email.android.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...