[MW:29955] RE: 29899] Material selection for Desalination plants and brinesolution

Dear Friend,

 

Stainless steels are the most widely used material in desalination plants. The ideal material for use in desalination plants is titanium because it suffers little to no corrosion in saltwater environments. However, titanium is far more expensive than stainless steels. There are advancements being made to improve the corrosion resistance of stainless steels. Highly alloyed ferritic and austenitic stainless steels are being tested in salt water in comparison to titanium. The stainless steels are normally alloyed with chromium, nickel, molybdenum, and nitrogen to improve their corrosion resistance.

 

Br

Dhanabal Jalachandran

 

Sent from Mail for Windows 10

 

From: Hrushikesh Sangamnerkar
Sent: 30 July 2019 18:38
To: Materials & Welding
Subject: [MW:29899] Material selection for Desalination plants and brinesolution

 

Dear expert,

 

Which material is suited to desalination plants keeping in mind the corrosion resistant properties?

 

Will titanium work well?

 

If any references or process licensors data available specifically for these applications do share.

 

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2oWhhDc7Db7kUtwjBrNNrZCuY7-nJ%3DLisuw0s80oup9Cw%40mail.gmail.com.

 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...