Wednesday, August 14, 2019

[MW:29951] Re: Material selection for Desalination plants and brine solution

Can use GRP / Rubber coated steel pipe.

On Tuesday, July 30, 2019 at 7:38:58 PM UTC+4, Hrushikesh Sangamnerkar wrote:
Dear expert,

Which material is suited to desalination plants keeping in mind the corrosion resistant properties?

Will titanium work well?

If any references or process licensors data available specifically for these applications do share.

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/83d2ab3c-27d0-48da-bf61-22201e71e208%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...