[MW:29932] Re: How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.



Hello ,
 
1 coupon for 2" OD pipe 60 is enough as per given in code  As per Sec.IX; QW303.2, 




Regards 

 

Sumit Bhadakwad
Welding & Piping inspector
Pune , India


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/980e17f0-1105-4601-bf55-ee713a12381c%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...