Re: [MW:29667] PIpe-Copper ASTM B466 UNS noC70600 & Fittings ASTM B151 UNS C70600

Dear Madhu,
You can use Er CuNi & E CuNi consumables for welding.
Testing as per sec IX are tensile and bend.

Regards,
Darshan

On Mon, 27 May 2019, 7:02 pm Madhu, <madhusudan.rout@gmail.com> wrote:
Dear Experts,

                    Please give your valuable feed back, I want to run the PQR, PQR as per ASME SEC-IX, What are testing requirement like mechanical , corrosion etc.
                   Suitable consumable,welding or brazing requirement &  Qualifying range?  its P NO-34 as per table.

                    PIpe-Copper ASTM B466 UNS noC70600 & Fittings ASTM B151 UNS C70600.

                    Please advice.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/df801094-e384-4cfe-9ea9-848524af3bb2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABDq6gh%3D%2Bqb88A697dZtCm92%2BdBGT1E4-OjbBp4N4%3DP%2BOpcjXg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...