Yes you can. You can also make weld repairs with your GTAW as long as you do not exceed the 2t qualified for your GTAW process which should be shown on your WPS.

On Thursday, June 13, 2019 at 1:23:35 PM UTC-5, panka...@gmail.com wrote:
Dear experts,
Can we do root by GTAW process, fillup by SMAW process and capping/final  by GTAW process?
Any precaution?
If no, why?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1f8d9578-c446-4efd-8895-492eac5ed2bd%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...