Re: [MW:29678] Charpy vee notch toughness

Dear ,

Its madatory to prepare if service temp is subzero, you may proceed with impact temp below by 5 c as per MDMT.

Regards

Dinesh

On Jun 2, 2019 9:42 PM, "Khaled lamraoui" <EURL.LHG@gmail.com> wrote:
Dear expert.                                  Please I need your help about the requirements of charpy vee notch toughness for piping and pipeline I mean when the test will be required.           I appreciate your help

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4adaf67b-388d-430d-bd1b-95ec89b8dc8f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrVd-f_E_0SBD7Dq9WTccSxTFN47i1%3DZS86ZMswWKJHuOw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...