John Henning explained very clear:

Yes you can.  However, if your WPS states that the filler metal per essential variable QW-404.5, will meet the Table QW-422 A-No. 1 chemistry limits, you will have to note that the Mn and Si must be 1.60 and 1.0 or less respectively.  You need to do incorporate this restriction as the SFA classification permits ER70-S6 to exceed the A-No. 1 limits

Confirmation on the AWS forum.Please check.

On Thursday, 6 June 2019, 14:40:41 GMT+3, George Dilintas <dilintas@gmail.com> wrote:


you cannot. No A number matches composition of ER7-S-6 becuase of Mn, You need a new PQR

Στις Δευ, 3 Ιουν 2019 στις 5:18 μ.μ., ο/η K K <karan.hbl@gmail.com> έγραψε:
Dear All,

My PQR is qualified with ER70S-2.

Can I use ( Mention) ER70S-6 in WPS.

Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/76403448-7204-4bda-83fd-21deebafcaa5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40B5phE-9QnFGCHmt4rxhEgAGs7fGZeynZygy5WyW3C_gg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...