Thursday, June 13, 2019

Re: [MW:29709] Welding consumable selection API 5L X80 M PSL2

any special requirements? pl. refer attachment


On Thu, 13 Jun 2019 at 16:26, 'PREM SHANKARDUTT NAUTIYAL' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi

Can some one please suggest what will be appropriate SMAW and SAW electrode/ wire for welding of following material #

API 5L X80 M PSL2

Regards

Prem Nautiyal


PREM S NAUTIYAL
CELL : 9769316004

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
--- 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmoSZ8%2BXq%3DHz1SH22uid%3Db3LE95wyf_PPcz4rOt3Hdbhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...