Re: [MW:29706] AISI 4130 and API 5CT Well Head Casing

Hi Ehab,
  1. E 10018-D2 - Electrode - SMAW
  2. ER 80S-D2 - FIller Wire - GTAW
You can use for SMAW first one.

Best Regards,

Venkat. G


On Wed, Jun 12, 2019 at 8:22 AM Ehab Ahmed <elpop102002@gmail.com> wrote:
Dear Sirs, 

Pleas help me to Select electrode ? for AISI 4130 (70-75 Ksi) and API 5CT L80 Pipe materials to weld by SMAW. 

Using ASME IX Code.  

Thanks and Best Regards,
Ehab Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20385728-b6dc-46fa-b65c-7fc06c8a7b47%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Venkatachalam Govindan
QHSE Lead / Trainer
(IRCA Registered Lead Auditor & API / CQI Practitioner)
+965 97604989, +919840502376 (
WhatsApp only)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3OcCQ0NZhMXx5OH-i_6UPZatxyms6%2BnYbYy%2BF5iqgJK2cg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...