[MW:29757] Increase of Carbon equivalent

Dear All,

Good day, 

Ref std :AWS D1.1
Material : EN 10025 275 JR to 275 JR.

We have qualified the PQR with CE 0.37. 
Now we are receiving the material having CE 0.39.
Please advise is it required additional PQR qualification.

Thanks
Kingsly Geo.V

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ-z1xagWgJXKvJSSnvr590zLape4B7MEzg%3Dba3o-%2BN2%3Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...