Dear All,

I have some Queries as below.

1) PQR is qualified with 1.6 mm diameter(filler wire), but sub vendor is mentioned 1.2 mm  and 1.6 mm diameter both in WPS.(  as per D1.1 Table 3.7 clause No- 7) A change in nominal electrode diameter(s) is essential Variables),How can they use 1.2 mm in WPS?

2) WPS and PQR base material using S275 JR but certificates are attached A36 material  - ( It's Acceptable as per code )

3) With reference to subject in WPS -  joint details - Backing and backgouging  - N/A. ( is it acceptable. )

Please clarify me regarding my above doubts.

Thanks in advance 

Regards
Kiran


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8dcf68e4-45b0-4d8b-8583-3f2d3f7a985d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...