Thursday, June 20, 2019

Re: [MW:29735] API 510 Inspection Interval


Api 510 inspection interval

If remaining life is 10 years or less
Inspection interval has it is.

If remaining life is greater than 10 years
1/2 of the life is inspection interval

If the remaining life is between 2 to 4 years 
Inspection interval is 2 years.

If the remaining life is less than 2 years
Full inspection interval. 



Please correct me if iam wrong

On Wed, 22 May 2019, 12:10 p.m. Raghu Raman, <raghuraman.ramasamy@gmail.com> wrote:
Hi Everyone,

A question related to Section 6.5 of API 510, Internal, On - Stream, and Thickness Measurement Inspections

When the remaining life is less than 4 years, the inspection interval may be the full remaining life up to a maximum of 2 years

Need help with this guys, what does it mean, my take is

if 3.5 years balance, inspection interval is 3.5 years

if 2.1 years balance, inspection interval is 2.1 years  

if 1.9 years balance, FFS takes over

Please correct, one concept i just cannot understand in the 510 exams

Thanks

Raghu Raman

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKqrTW0sMMi7VqF2CCUVOyTA1GKfCgVrAQBQdunncF6JMFt_bA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_yh8oTLtzWOpf1c8fPmbBYcqRxZk%3DBM8Ffb_c_3eB_WP-Cxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...