Most fabricators select ER80S-D2 filler rod, which produces welds with a high tensile strength ( note, consider that S-2 fillers clean impurities better than D-2 fillers). In any event, do not use 4130 filler, as the weld will not have sufficient ductility unless it undergoes stress relief. 
On Saturday, June 8, 2019 at 10:53:22 AM UTC-5, Venkat QMR (IRCA, Lead Auditor)) wrote:
Dear Sirs,

Anyone can help me to explain the method of electrode selection? for AISI 4130 and A681 L6 materials to weld for repair.

Also, please write about normal practice? 

Thanks and Best Regards,

Venkat. G

--
Venkatachalam Govindan
QHSE Lead / Trainer
(IRCA Registered Lead Auditor & API / CQI Practitioner)
+965 97604989, +919840502376 (
WhatsApp only)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bd9f75c3-d123-4453-b0f4-8cb8a779ba97%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...