Tuesday, June 18, 2019

Re: [MW:29724] Aluminium bronze to CuNi 90/10 base metal welding

use ER CuAl-A2

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Jun 18, 2019 at 3:29 PM Rahul Rathod <welder.tigarc6g@gmail.com> wrote:
Dear Experts,
Greetings!
Which welding consumables Is good for aluminium bronze to CuNi 90/10 base metal Welding? Recently we used CuNi 90/10 but we observed crack in weld metal, your positive reply is so valuable to us.

With Regards


Rahul J Rathod 
Welding Technician 

What's up +9181155889118?

 view my profile onLinkedIn view my profile on facebook my skype id

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANaNbfm9NPR%2BceeQvvsFt2-rtyRbedQnQ3d8b6NOiWsQobK2Cg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN1JdrRESuppg6-4bDJsp4kXQVEem8B3_fQjK-EXjA%3Dww%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...